Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115.2 MPa
16710 psi
ASTM D638
Elongation at Break 1.44 %
1.44 %
ASTM D638
Tensile Modulus 12.42 GPa
1801 ksi
ASTM D638
Flexural Yield Strength 182.7 MPa
26500 psi
ASTM D790
Flexural Modulus 10.4 GPa
1510 ksi
ASTM D790
Compressive Yield Strength 160.7 MPa
23310 psi
ASTM D695
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 2.50e+16 ohm-cm
2.50e+16 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
Short Time; ASTM D149
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 20 sec
20 sec
ASTM D495
Comparative Tracking Index 225 V
225 V
ASTM D3638
Users viewing this material also viewed the following: