Material Notes:
PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component file E40654. 07200 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.550 g/cc
0.0199 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.43 %
0.43 %
ASTM D570
Linear Mold Shrinkage 0.0106 cm/cm
0.0106 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 0.67 %
0.67 %
ASTM D638
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Flexural Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 6.20 GPa
899 ksi
ASTM D790
Compressive Strength 188 MPa
27300 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 2.87 GPa
416 ksi
Calculated
Izod Impact, Notched 0.208 J/cm
0.390 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.194 J/cm²
0.923 ft-lb/in²
ASTM D256
Impact 148
148
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.350 W/m-K

@Temperature 100 °C
2.43 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 187 °C
369 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
298 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 27.2 %
27.2 %
ASTM D2863
Shrinkage 0.47 %
0.47 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+11 ohm-cm
1.40e+11 ohm-cm
ASTM D247
Dielectric Constant 5.4
5.4
ASTM D150
Dielectric Strength 7.10 kV/mm
180 kV/in
Short Time; ASTM D149
Dissipation Factor 0.067
0.067
ASTM D150
Arc Resistance 119 sec
119 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638
Users viewing this material also viewed the following: