PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer PolyOne Corporation
Trade Name Bergamid™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
±0.03 g/cm³; DIN 53479
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
ISO 527-2/50
Elongation at Yield 22 %

@Temperature 23.0 °C
22 %

@Temperature 73.4 °F
ISO 527-2/50
Tensile Modulus 1.10 GPa

@Temperature 23.0 °C
160 ksi

@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
13.0 J/cm²

@Temperature 23.0 °C
61.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
ISO 3146
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous (GTP 50% Tensile); IEC 60216
175 °C
347 °F
Short Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Unannealed; ISO 75-2/A
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 7.0

@Frequency 1.00e+6 Hz
7.0

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 60.0 kV/mm
1520 kV/in
IEC 60243-1
Dissipation Factor 0.30

@Frequency 1.00e+6 Hz
0.30

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Descriptive Properties Value Comments
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
K-Value 74.0 to 78.0
No Standard; 96% H2SO4
Regional Availability Africa & Middle East
Asia Pacific
Europe
RoHS Compliance RoHS Compliant