Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ES-20GF/000 Polyethersulfone, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Tensile Strength, Ultimate 124 MPa
18000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 5.86 GPa
850 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.40 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.9 µm/m-°C

@Temperature 20.0 °C
14.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Annealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257