Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Melt Flow 2.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 100 %
100 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C

@Thickness 1.57 mm
185 °F

@Thickness 0.0618 in
Annealed; ASTM D648
Flammability, UL94 V-0
V-0
UL 94
Descriptive Properties Value Comments
Features Flame Retardant
Medium Impact Resistance
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)