Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
ASTM D955
Melt Flow 2.7 - 6.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.7 - 6.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 10 %
10 %
Type I, 51 mm/min; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.210 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.393 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.2 °C

@Thickness 3.18 mm
198 °F

@Thickness 0.125 in
Unannealed; ASTM D648
UL RTI, Electrical 105 °C
221 °F
UL 746
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
NC; UL 94
Processing Properties Metric English Comments
Mold Temperature 16.0 - 50.0 °C
60.8 - 122 °F
Descriptive Properties Value Comments
Additive Heat Stabilizer
Features Heat Stabilized
Medium Flow
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following: