Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek RA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% glass fiber reinforced, self extinguishing halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
DIN 53479
Water Absorption 6.0 %
6.0 %
DIN 53495
Moisture Absorption at Equilibrium 1.9 %
1.9 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM-D785
Tensile Strength, Yield 120 MPa
17400 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM-D790
Izod Impact, Notched 0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 120 °C
248 °F
Continuous Use
240 °C
464 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
DIN 53461
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
DIN 53482
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 80.0 kV/mm
2030 kV/in
VDE 0303/4
Users viewing this material also viewed the following: