Material Notes:
Impact modified, UV and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
DIN 53479
Water Absorption 6.0 %
6.0 %
DIN 53495
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM-D785
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM-D638
Elongation at Break 20 %
20 %
ASTM-D638
Flexural Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM-D790
Izod Impact, Notched 2.50 J/cm

@Temperature 23.0 °C
4.68 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
>= 180 °C
>= 356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 90.0 kV/mm
2290 kV/in
VDE 0303/4