Polyram PlusTek RB703 Nylon 6, UV Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RB703 Nylon 6, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose, UV stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Moisture Absorption at Equilibrium 1.3 %
1.3 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 70.0 MPa
>= 10200 psi
ASTM-D638
Elongation at Break >= 15 %
>= 15 %
ASTM-D638
Flexural Strength >= 95.0 MPa
>= 13800 psi
ASTM D790
Flexural Modulus >= 2.20 GPa
>= 319 ksi
ASTM-D790
Izod Impact, Notched >= 0.600 J/cm

@Temperature 23.0 °C
>= 1.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 160 °C
>= 320 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) >= 65.0 °C
>= 149 °F
DIN 53461