Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP YI001 Polyester Elastomer (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP YI001 Polyester Elastomer (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* YI001 is a compound based on Polyester Elastomer containing Silicone. Added features include; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.021 cm/cm
0.021 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa
2030 psi
50 mm/min; ISO 527
Elongation at Yield 37 %
37 %
50 mm/min; ISO 527
Tensile Modulus 0.180 GPa
26.1 ksi
1 mm/min; ISO 527
Flexural Strength 9.00 MPa
1310 psi
2 mm/min; ISO 178
Flexural Yield Strength 12.0 MPa
1740 psi
2 mm/min; ISO 178
Flexural Modulus 0.180 GPa
26.1 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 200 µm/m-°C

@Temperature 23.0 - 60.0 °C
111 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 216 µm/m-°C

@Temperature 23.0 - 60.0 °C
120 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 193 °C
379 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af