Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 94.0 MPa
13600 psi
5 mm/min; ISO 527
Elongation at Break 3.5 %
3.5 %
5 mm/min; ISO 527
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
Flexural Yield Strength 134 MPa
19400 psi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 38.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 170 µm/m-°C

@Temperature 23.0 - 60.0 °C
94.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Copyright © lookpolymers.com All Rights Reserved