Sapco C 410 Steatite

Category Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer Sapco
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sapco C 410 Steatite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sapco.
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Open Porosity <= 0.50 %
<= 0.50 %
Mechanical Properties Metric English Comments
Modulus of Elasticity 65.0 GPa
9430 ksi
Flexural Strength 50.0 MPa
7250 psi
Compressive Strength 300 MPa
43500 psi
Thermal Properties Metric English Comments
CTE, linear 3.00 µm/m-°C

@Temperature 20.0 °C
1.67 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.900 J/g-°C
0.215 BTU/lb-°F
Thermal Conductivity 2.10 W/m-K
14.6 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1000 °C
1830 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm