Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 2.88e+14 ohm-cm Grade Count:12 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 9.59e+15 ohm-cm Grade Count:19 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 7.97e+15 ohm-cm Grade Count:40 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Electrical Resistivity | 1.00e+11 - 7.00e+13 ohm-cm | 1.00e+11 - 7.00e+13 ohm-cm | Average value: 2.67e+13 ohm-cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 93 |
Solvay Technyl® C 206 Nylon 6, EH50 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 93 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 500 °C |
1.00e+11 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 65.0 °C |
1.00e+11 ohm-cm @Temperature 149 °F |
Insulation Resistance During 10th day Cycling (95% Relative Humidity) |
Cytec Conathane® CE-1163 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 9.17e+13 ohm-cm Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 8.78e+13 ohm-cm Grade Count:6 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |