Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 1.03e+16 ohm-cm Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+16 ohm-cm | 1.00e+11 - 1.00e+16 ohm-cm | Average value: 7.78e+15 ohm-cm Grade Count:9 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 1.06e+14 ohm-cm Grade Count:11 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+13 ohm-cm | 1.00e+11 - 1.00e+13 ohm-cm | Average value: 4.26e+12 ohm-cm Grade Count:15 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+11 - 2.10e+14 ohm-cm | 1.00e+11 - 2.10e+14 ohm-cm | Average value: 1.05e+13 ohm-cm Grade Count:26 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 2.88e+14 ohm-cm Grade Count:12 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 9.59e+15 ohm-cm Grade Count:19 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Electrical Resistivity | 1.00e+11 - 7.00e+13 ohm-cm | 1.00e+11 - 7.00e+13 ohm-cm | Average value: 2.67e+13 ohm-cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+13 ohm-cm | 1.00e+11 - 1.00e+13 ohm-cm | Average value: 3.70e+12 ohm-cm Grade Count:3 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 93 |
Solvay Technyl® C 206 Nylon 6, EH50 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 93 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 500 °C |
1.00e+11 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 9.17e+13 ohm-cm Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |