Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber

Category Polymer , Thermoplastic , Polysulfone (PSU) , Polysulfone, 10% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Udel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the polysulfone resin. The high performance properties and attractive price make these resins particularly effective alternatives to metals in many engineering applications.Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Strength; High Heat Resistance; High Rigidity; Hydrocarbon Resistant; Hydrolytically StableUses: Appliance Components; Appliances; Automotive Electronics; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Parts; Microwave Cookware; Piping; Plumbing Parts; Valves/Valve PartsInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 343 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 108 MPa
15700 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 8.69 GPa
1260 ksi
ASTM D638
Flexural Strength 154 MPa
22300 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Tensile Impact Strength 113 kJ/m²
53.8 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 181 °C
358 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 3.18 mm
V-0

@Thickness 0.125 in
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.47

@Frequency 1.00e+6 Hz
3.47

@Frequency 1.00e+6 Hz
ASTM D150
3.48

@Frequency 60.0 Hz
3.48

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Dissipation Factor 0.00070

@Frequency 60.0 Hz
0.00070

@Frequency 60.0 Hz
ASTM D150
0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
NSF Yes
Yes
NSF 61
Processing Properties Metric English Comments
Melt Temperature 343 - 399 °C
649 - 750 °F
Mold Temperature 121 - 163 °C
250 - 325 °F
Drying Temperature 163 - 191 °C

@Time 10800 - 14400 sec
325 - 376 °F

@Time 3.00 - 4.00 hour
Back Pressure 0.345 - 0.689 MPa
50.0 - 99.9 psi
Descriptive Properties Value Comments
Agency Ratings ISO 10993; ISO 10993-Part 1
Availability Asia Pacific
Europe
Latin America
North America
Color Black; Natural; Opaque
Form Pellets
Injection Rate Fast
Processing Technique Extrusion; Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.0:1.0
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved