Solvay TECHNYL® C 206 PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 206 PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored by a high crystallization rate. It is especially suitable for the production of technical moldings with fast injection cycles. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527 type 1 A
Tensile Modulus 1.10 GPa
160 ksi
ISO 527 Type 1A
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 3.9
3.9
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243
Dissipation Factor 0.10
0.10
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %