Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
4.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-1200 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-2000 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | |
Reliance Industries Polypropylene - Talc filled Information provided by Reliance Industries |
|||
Izod Impact, Unnotched | 2.40 - 5340 J/cm | 4.50 - 10000 ft-lb/in | Average value: 6.94 J/cm Grade Count:13 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 2.40 J/cm - NB | 4.50 ft-lb/in - NB | Average value: 6.74 J/cm Grade Count:91 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Unnotched | 2.40 - 10.7 J/cm | 4.50 - 20.0 ft-lb/in | Average value: 6.27 J/cm Grade Count:31 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 2.40 - 2.80 J/cm @Temperature 23.0 °C |
4.50 - 5.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 210/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS SS7 MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM HO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Izod Impact, Unnotched | 2.40 - 13.3 J/cm | 4.50 - 25.0 ft-lb/in | Average value: 5.97 J/cm Grade Count:14 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Temperature 23.0 °C |
4.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp GZL34E PSU LNP LUBRICOMP* GZL34E is a compound based on Polysulfone resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend. |