Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Styrolux® GH 58 SBC

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Styrolution
Trade Name Styrolux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Styrolux® GH 58 SBC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Styrolux® GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance for general molding applications. Styroclear GH 58 may be suitable for conventional thermoplastics processing technologies such as injection molding.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Melt Flow 16 g/10 min
16 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ASTM D2240
Tensile Strength, Yield 28.0 MPa
4060 psi
2in/min; ASTM D638
Elongation at Break 43 %
43 %
ASTM D638
Tensile Modulus 1.68 GPa
244 ksi
2in/min; ASTM D882
Flexural Strength 33.0 MPa
4790 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Dart Drop, Total Energy 0.600 J
0.443 ft-lb
Total energy; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM D648
Vicat Softening Point 90.0 °C

@Load 1.02 kg,
Temperature 120 °C
194 °F

@Load 2.25 lb,
Temperature 248 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 180 - 235 °C
356 - 455 °F
Injection
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Descriptive Properties Value Comments
Commercial Status North America
Copyright © lookpolymers.com All Rights Reserved