Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Mineral/Fiber Filled
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Durez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical and appliance applications.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Water Absorption 0.40 %
0.40 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Tensile Modulus 10.3 GPa
1490 ksi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
Compressive Strength 179 MPa
26000 psi
ASTM D695
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
UL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.00 mm
V-1

@Thickness 0.0394 in
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 5.0

@Frequency 1e+6 Hz
5.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
Step by step; ASTM D149
14.7 kV/mm
373 kV/in
Short Time; ASTM D149
Dissipation Factor 0.040

@Frequency 1e+6 Hz
0.040

@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 225 V
225 V