Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade

Category Polymer , Thermoset , Phenolic
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Durez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimensional tolerance, impact strength, and other properties required in pulley applications.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Apparent Bulk Density 0.490 g/cc
0.0177 lb/in³
ASTM D1895
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Tensile Modulus 6.90 GPa
1000 ksi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
Compressive Strength 207 MPa
30000 psi
ASTM D695
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature 30.0 - 150 °C
20.0 µin/in-°F

@Temperature 86.0 - 302 °F
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Thermal Conductivity 0.370 W/m-K
2.57 BTU-in/hr-ft²-°F
Cenco Fitch
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 5.1

@Frequency 1e+6 Hz
5.1

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
Step by step; ASTM D149
12.8 kV/mm
325 kV/in
Short Time; ASTM D149
Dissipation Factor 0.050

@Frequency 1e+6 Hz
0.050

@Frequency 1e+6 Hz
ASTM D150