TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0Iceberg Clay75.0Coumarone-Indene Resin25.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
Mooney Viscosity 21

@Temperature 121 °C
21

@Temperature 250 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
Tensile Strength, Yield 17.9 MPa
2600 psi
Elongation at Yield 650 %
650 %
100% Modulus 0.00276 GPa
0.400 ksi
300% Modulus 0.00689 GPa
1.00 ksi
Tear Strength 43.0 kN/m
245 pli
Graves
Compression Set 27 %
27 %
Method B
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 142 °C
1.50 hour

@Temperature 287 °F