Material Notes:
Availability: North AmericaForms: PelletsUL File Number: E157318Appearance: Red8661111Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 126 µm/m-°C
70.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+15 ohm-cm
3.00e+15 ohm-cm
ASTM D257
Dielectric Strength 16.1 kV/mm
410 kV/in
Method A (Short-Time); ASTM D149