Techmer Lehvoss Compounds Luvotech™ J-1305/40 BK5011 PPS  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer Lehvoss Compounds Luvotech™ J-1305/40 BK5011 PPS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Physical Properties Metric English Comments
Specific Gravity 1.67 g/cc
1.67 g/cc
ASTM D792
Water Absorption 0.020 %
0.020 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 159 MPa
23000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 221 MPa
32000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in