Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQTENE® 2003 PBK 41 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2003 PBK 41 is a black compound especially developed for irrigation pipe. LACQTENE® 2003 PBK 41 may be used geomembranes.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
200°C; EN 728
Melt Flow 0.20 g/10 min

@Load 2.16 kg
0.20 g/10 min

@Load 4.76 lb
ISO 1133
0.75 g/10 min

@Load 5.00 kg
0.75 g/10 min

@Load 11.0 lb
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 868
Tensile Strength, Yield 19.0 MPa
2760 psi
ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Flexural Modulus 0.750 GPa
109 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
ISO 3146
Vicat Softening Point 118 °C
244 °F
ISO 306
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.