Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumicene® mPE M 4041 UV is a new generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 4041 UV is intended for the manufacture of rotomolded items.Lumicene® mPE M 4041 UV is a natural grade available in pellets form.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133/D
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.0 MPa
3050 psi
ISO 527-2
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527-2
Elongation at Break >= 800 %
>= 800 %
ISO 527-2
Elongation at Yield 11 %
11 %
ISO 527-2
Flexural Modulus 0.730 GPa
106 ksi
ISO 178
Charpy Impact, Notched >= 15.0 J/cm²

@Temperature 23.0 °C
>= 71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1
>= 15.0 J/cm²

@Temperature -30.0 °C
>= 71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179-1
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ISO 11357