Material Notes:
TRA-BOND 400-5 adhesive is a general purpose non-conductive epoxy. It combines the properties of a moderate work life with the ability to cure rapidly at temperatures as low as 60°C. Having a relatively low viscosity, TRA-BOND 400-5 adhesive is well suited for use in wet coil winding applications.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 3500 cP

@Temperature 25.0 °C
3500 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 14.5 MPa
2100 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 115 °C
239 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 150 °C
0.0333 hour

@Temperature 302 °F
5.00 min

@Temperature 125 °C
0.0833 hour

@Temperature 257 °F
30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
60.0 min

@Temperature 75.0 °C
1.00 hour

@Temperature 167 °F
120 min

@Temperature 60.0 °C
2.00 hour

@Temperature 140 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Thixotropic Index 1
Working Life hours 4
At 25°C