Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Bond FDA25 Food and Drug Application Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FDA25 Food and Drug Application Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FDA-25 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administration Chapter 1, Sub Part B, Sections 175.105 and 175.300. This two-part adhesive is commonly used for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND FDA-25 is an effective electrical insulator, and it provides low permeability to gases and vapors and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mixed
Volatile Organic Compounds (VOC) Content 7.12 g/l
7.12 g/l
Water Absorption 0.16 %
0.16 %
After 24 hours
Viscosity 28500 cP

@Temperature 25.0 °C
28500 cP

@Temperature 77.0 °F
Mixed (rv #6, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Adhesive Bond Strength 16.5 MPa
2400 psi
Lap shear, alum to alum, 1 hr @ 65°C
18.3 MPa
2650 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 89.9 µm/m-°C
49.9 µin/in-°F
Below Tg
218 µm/m-°C
121 µin/in-°F
Above Tg
Maximum Service Temperature, Air 140 °C
284 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 125 °C
257 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Pot Life 25 min
25 min
100 grams
30 min
30 min
25 grams
Descriptive Properties Value Comments
Color Black
Mix Ratio, parts by weight 100/23
Resin/Hardener
Thixotropic Index 2
5 rpm/50 rpm
Users viewing this material also viewed the following: