Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® B 97 Heat Cure Catalyst

Category Polymer , Adhesive , Thermoset
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® B 97 Heat Cure Catalyst.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming B 97 Eccobond® Heat Cure CatalystVery high temperature resistance, not as brittle as 17 M 1. Cures from 80°C to 200°C. Excellent chemical resistance. May also be used as an accelerator for 17 M 1. Long working life. Cured castings exhibit excellent retention of properties at elevated temperatures and outstanding chemical resistance. Cure Type: Heat
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
Viscosity 4000 - 8000 cP

@Temperature 25.0 °C
4000 - 8000 cP

@Temperature 77.0 °F
Mixed
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 150 °C
1.00 - 4.00 hour

@Temperature 302 °F
240 min

@Temperature 60.0 °C
4.00 hour

@Temperature 140 °F
Pot Life >= 1440 min

@Temperature 25.0 °C
>= 1440 min

@Temperature 77.0 °F
100 grams
Descriptive Properties Value Comments
Color Reddish Brown
Users viewing this material also viewed the following: