Material Notes:
Extrusion and pipe applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
ESCR 100% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
ASTM D1693
Carbon Black Loading 2.4 %
2.4 %
ISO 6469
Melt Flow 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
Elongation at Yield 7.0 %
7.0 %
ISO 527
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Charpy Impact, Notched 0.110 J/cm²

@Temperature 23.0 °C
0.524 ft-lb/in²

@Temperature 73.4 °F
ISO 179
0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 116 °C
241 °F
ISO 306
Users viewing this material also viewed the following: