Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
GB/1033
Water Absorption 0.70 %
0.70 %
23°C•24h
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
GB/15585
Mechanical Properties Metric English Comments
Tensile Strength, Yield 78.0 MPa
11300 psi
GB/1040
Flexural Strength 124 MPa
18000 psi
GB/9341
Charpy Impact Unnotched 2.20 J/cm²
10.5 ft-lb/in²
IS0179-1:2000
Charpy Impact, Notched 0.520 J/cm²
2.47 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
GB1634
Flammability, UL94 V-0
V-0
GB/T2408
Flammability Test 20
20
Flame Remainder (%); GB/9345
Electrical Properties Metric English Comments
Comparative Tracking Index 350 V
350 V
GB/4207
Processing Properties Metric English Comments
Processing Temperature 255 - 280 °C
491 - 536 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 110 °C

@Time 7200 sec
230 °F

@Time 2.00 hour
Vacuum Pressure, -0.08 MPa
120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Chute Hot-Wind
120 °C

@Time 21600 sec
248 °F

@Time 6.00 hour
Horizontal Oven
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Descriptive Properties Value Comments
Speed of Shoot, % 35-95
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved