Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate

Category Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
Relative Density; ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Compression Molding; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 69.0 MPa
10000 psi
ASTM D638
Flexural Strength 110 MPa
16000 psi
At Rupture; ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Compressive Strength 131 MPa
19000 psi
ASTM D695
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Thermal Conductivity 0.360 W/m-K
2.50 BTU-in/hr-ft²-°F
ASTM C-518
Maximum Service Temperature, Air 130 °C
266 °F
UL 746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
As molded; ASTM D648
Oxygen Index 29 %
29 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
Wet; ASTM D150
3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
wet; ASTM D150
Dielectric Strength 14.8 kV/mm
376 kV/in
60Hz, Step-by-Step, wet; ASTM D149
Dissipation Factor 0.011

@Frequency 1000 Hz
0.011

@Frequency 1000 Hz
wet; ASTM D150
0.014

@Frequency 1e+6 Hz
0.014

@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 175 sec
175 sec
ASTM D495
Comparative Tracking Index >= 600 V
>= 600 V
IEC 112
Descriptive Properties Value Comments
Color Black, Blue, Brown, Green, Red, White
Form Granular
Main Filler Glass Fiber
Molding Method Compression, transfer, injection