Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Zhejiang Double Fish Plastics Co., Ltd
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, communications (bobbin, relay bed, optical cable closure), military, sports equipment (skis, helmets, foot wear), and medical equipment. Product is customizable.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Filler Content 50 %
50 %
Glass Fiber
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 135 MPa
19600 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Flexural Strength 185 MPa
26800 psi
ASTM D790
Flexural Modulus 8.90 GPa
1290 ksi
ASTM D790
Izod Impact Resistance 3.20 J/cm²
15.2 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
324 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 216 - 232 °C
421 - 450 °F
Middle Barrel Temperature 210 - 227 °C
410 - 441 °F
Front Barrel Temperature 204 - 221 °C
399 - 430 °F
Melt Temperature 210 - 249 °C
410 - 480 °F
Mold Temperature 38.0 - 77.0 °C
100 - 171 °F
Injection Velocity 13.0 - 25.0 mm/sec
0.512 - 0.984 in/sec
Injection Pressure 69.0 - 103 MPa
10000 - 14900 psi
Hold Pressure 34.0 - 69.0 MPa
4930 - 10000 psi
Back Pressure 0.170 - 0.340 MPa
24.7 - 49.3 psi
Screw Speed 30 - 70 rpm
30 - 70 rpm