Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 240 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 230 - 240 °C
446 - 464 °F
Blow Molding
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET  (Unverified Data**)
Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme..
Melt Temperature 210 - 240 °C
410 - 464 °F
Extrusion
Polimeri Europa Edistir N 2380 Polystyrene
High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla..
Melt Temperature 200 - 240 °C
392 - 464 °F
Total Lacqrene® 4240(AS) High Impact Polystyrene  (discontinued **)
LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi..
Melt Temperature 230 - 240 °C
446 - 464 °F
Eastman Tenite 358-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Melt Temperature 210 - 240 °C
410 - 464 °F
Injection Molding
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Melt Temperature 210 - 240 °C
410 - 464 °F
Injection Molding
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Melt Temperature 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
Melt Temperature 220 - 240 °C
428 - 464 °F
LG Chemical LUPOS GP-2201F General Purpose ABS, 20% Glass Fiber Reinforced, Flame Retardant
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Melt Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by ..
Melt Temperature 220 - 240 °C
428 - 464 °F
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Melt Temperature 200 - 240 °C
392 - 464 °F
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Melt Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
Melt Temperature 200 - 240 °C
392 - 464 °F
LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov..
Melt Temperature 200 - 240 °C
392 - 464 °F
ISO 294
Styrolution Novodur® BX13036 ABS + PMMA
Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution
Melt Temperature 200 - 240 °C
392 - 464 °F
Flat film
Styrolution Polystyrol 143 E GR 2 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
Melt Temperature 200 - 240 °C
392 - 464 °F
Flat film
Styrolution Polystyrol ESCRimo PS
Description: Polystyrol ESCRimo is a high-impact polystyrene grade with an improved stress cracking resistance compared to conventional high-impact polystyrene.Applications: Due to its superior envi..
Melt Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 220 - 240 °C
428 - 464 °F
Tisan TISLAMID® 6 20% Glass Fiber Reinforced, Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melt Temperature 220 - 240 °C
428 - 464 °F
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melt Temperature 220 - 240 °C
428 - 464 °F
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melt Temperature 220 - 240 °C
428 - 464 °F
Covestro Desmopan® DP 9662DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro..
Melt Temperature 230 - 240 °C
446 - 464 °F
DAM; Extrusion
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6  (Unverified Data**)
Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In..
Melt Temperature 230 - 240 °C
446 - 464 °F
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
Melt Temperature 220 - 240 °C
428 - 464 °F
LATI Latimass 53-04 D009 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Melt Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR401F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical
Melt Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR404T ABS, Heat Resistance
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical..
Copyright © lookpolymers.com All Rights Reserved