| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
Plastcom PLASTAMID® 66 BT B 27 A PA66
PA66 for compounding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, h..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Polimeri Europa Sinkral® E 332 ABS Resin
Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Polykemi AB POLYblend C65F PC/ABS-blend
Information provided by Polykemi AB
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | Injection Molding |
|
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**)
Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Do not melt above 300°C |
|
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 250°C |
|
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation..
|
|||
| Melt Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical Lupox® GP1000S PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical Lupox® GP1000W PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
|
Ineos ABS Lustran® M210TF ABS Pellets
Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo..
|
|||
| Melt Temperature | 240 - 290 °C | 464 - 554 °F | |
|
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
LATI Laticonther 83 CP/80 PA12, Impact Modified
High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
LATI Latiohm 63-08 PD02 G/25 PA6, 25% Glass Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6), impact modified. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Injection |
|
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
|
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
|
|||
| Melt Temperature | 240 - 290 °C | 464 - 554 °F | |
|
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
|
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960..
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
|
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
|
Covestro Bayblend® FR 3011 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradegood flowhigh heat resistanceVicat/B 120 temperature = 118 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Covestro Bayblend® W85 XF* Polycarbonate + ASA
Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film
Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck..
|
|||
| Melt Temperature | 240 °C | 464 °F | Optimum; Extrusion |
|
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont
|
|||