| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | A. Schulman, Inc. |
| Trade Name | SCHULAMID® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
| Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.175 mm |
0.0080 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 3.45 MPa | 500 psi | ISO 527 |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ISO 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 190 °C | 374 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | ISO 75 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
| Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
| Drying Temperature | 79.4 °C | 175 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
| Moisture Content | 0.080 - 0.12 % | 0.080 - 0.12 % |