Polymer Property : Dielectric Strength = 1020 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
IEC 60243-1
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
IEC 60243-1
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
IEC 60250
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
IEC 60243-1
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Dielectric Strength 27.0 - 40.0 kV/mm
686 - 1020 kV/in
Average value: 31.3 kV/mm Grade Count:11
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Dielectric Strength 25.6 - 40.0 kV/mm
650 - 1020 kV/in
Average value: 33.3 kV/mm Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Dielectric Strength 20.0 - 40.0 kV/mm

@Thickness 0.800 - 3.20 mm
508 - 1020 kV/in

@Thickness 0.0315 - 0.126 in
Average value: 27.6 kV/mm Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Dielectric Strength 25.0 - 40.0 kV/mm
635 - 1020 kV/in
Average value: 31.6 kV/mm Grade Count:10
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Dielectric Strength 15.7 - 40.0 kV/mm
400 - 1020 kV/in
Average value: 24.5 kV/mm Grade Count:33
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Dielectric Strength 20.0 - 40.0 kV/mm

@Thickness 2.00 mm
508 - 1020 kV/in

@Thickness 0.0787 in
IEC 60243
Manifattura Cattaneo PVC U Polyvinyl Chloride
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Dielectric Strength 20.0 - 40.0 kV/mm
508 - 1020 kV/in
VDE 0303
GEHR Plastics Corzan® PVC-C Polyvinylchloride
Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou..
Dielectric Strength 20.0 - 40.0 kV/mm
508 - 1020 kV/in
ASTM D149/15
Mikro-Technik Reproflon PTFE
Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
ASTM D149
Guarniflon MFA Fluoropolymer
It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It ..
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
ASTM D149
Guarniflon PFA Perfluoroalkoxy Polymer
Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli..
Dielectric Strength 35.0 - 40.0 kV/mm

@Thickness 1.00 mm
889 - 1020 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer
Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re..
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
Dielectric Strength 25.0 - 40.0 kV/mm
635 - 1020 kV/in
ASTM D149
Adamas Adalon® 415 PTFE, 10% Organic Filler
Information provided by Adamas, HPM
Dielectric Strength 25.0 - 40.0 kV/mm
635 - 1020 kV/in
ASTM D149
Adamas Adalon® 433 PTFE, 10% Ekonol®
Information provided by Adamas, HPM
Dielectric Strength 25.0 - 40.0 kV/mm
635 - 1020 kV/in
ASTM D149
Adamas Adalon® 436 PTFE, 15% Ekonol®
Information provided by Adamas, HPM
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, ..
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Dielectric Strength 16.5 - 40.0 kV/mm
420 - 1020 kV/in
Average value: 27.6 kV/mm Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Dielectric Strength 19.7 - 40.0 kV/mm
500 - 1020 kV/in
Average value: 29.2 kV/mm Grade Count:13
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
IEC 60243-1
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
Dielectric Strength 20.0 - 40.0 kV/mm
508 - 1020 kV/in
Average value: 27.0 kV/mm Grade Count:18
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Dielectric Strength 19.3 - 40.0 kV/mm
490 - 1020 kV/in
Average value: 25.1 kV/mm Grade Count:28
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Dielectric Strength 17.7 - 40.0 kV/mm
450 - 1020 kV/in
Average value: 25.9 kV/mm Grade Count:24
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..