| Special Metals BRIGHTRAY® Alloy B Electrical Resistance Alloy | 
        Electronic/Magnetic Alloy | 
        		BRIGHTRAY®
		 | 
      
            
        | Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy | 
        Electronic/Magnetic Alloy | 
        		BRIGHTRAY®
		 | 
      
            
        | Special Metals BRIGHTRAY® Alloy S Electrical Resistance Alloy | 
        Electronic/Magnetic Alloy | 
        		BRIGHTRAY®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged | 
        Nickel Alloy | 
        		DURANICKEL®
		 | 
      
            
        | Special Metals Electroformed Nickel, 100 Micron (4 mil) Foil, As-Electroformed | 
        Pure Element | 
         | 
      
            
        | Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed | 
        Pure Element | 
         | 
      
            
        | Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed | 
        Pure Element | 
         | 
      
            
        | Special Metals Electroformed Nickel, 6 Micron (0.24 mil) Foil, As-Electroformed | 
        Pure Element | 
         | 
      
            
        | Special Metals FERRY® Alloy | 
        Superalloy | 
        		FERRY®
		 | 
      
            
        | Special Metals INCOLOY® Alloy 825 | 
        Superalloy | 
        		INCOLOY®
		 | 
      
            
        | Special Metals INCOLOY® alloy 864 | 
        Nickel Alloy | 
        		INCOLOY®
		 | 
      
            
        | Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy | 
        Superalloy | 
        		INCOLOY®
		 | 
      
            
        | Special Metals INCOLOY® Alloy 925 | 
        Superalloy | 
        		INCOLOY®
		 | 
      
            
        | Special Metals INCONEL® 601GC® Nickel Superalloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 10% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 15% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 20% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 30% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 40% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 50% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C) + Aged 1400°F (760°C) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) + Aged 1200°F (650°C) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) + Aged 1400°F (760°C) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.250 in (6.4 mm) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.500 in (12.7 mm) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.50 inch (12.7 mm) o.d. and 0.050 inch (1.27 mm) Thickness | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.75 inch (19.0 mm) o.d. and 0.065 inch (1.65 mm) Thickness | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.5 x 2.0 inch (13 x 51 mm) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 2 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, Solution Treated | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, 2 Part Heat Treatment | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, 3 Part Heat Treatment | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, Solution Treated | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Flat, 2 Part Heat Treatment, 1.250 inch (31.8 mm) Thickness | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 3 Part Heat Treatment, 8.0 inch (203 mm) Diameter | 
        Iron Base | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725) Age Hardened Strip | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Tube | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® alloy 22 Austenitic Alloy | 
        Nickel Alloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy 600 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy 601 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy 617 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy 625 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® alloy 693 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy 718 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy 751 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy C-276 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy G-3 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy MA 754 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® Alloy X-750 | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Bar | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Plate | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Sheet | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed) | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® G-3 Nickel Superalloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® HX Nickel Superalloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy | 
        Superalloy | 
        		INCONEL®
		 | 
      
            
        | Special Metals MONEL® 404 Copper-Nickel Alloy | 
        Nickel Alloy | 
        		MONEL®
		 | 
      
            
        | Special Metals MONEL® Alloy 400 | 
        Superalloy | 
        		MONEL®
		 | 
      
            
        | Special Metals MONEL® Alloy 401 | 
        Superalloy | 
        		MONEL®
		 | 
      
            
        | Special Metals MONEL® Alloy K-500 | 
        Superalloy | 
        		MONEL®
		 | 
      
            
        | Special Metals MONEL® Alloy R-405 | 
        Superalloy | 
        		MONEL®
		 |