3M Scotchcal™ ElectroCut™ 7725-98 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name Scotchcal™ ElectroCut™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcal™ ElectroCut™ 7725-98 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier assembly of multi-color graphics; Superior cutting as small as 0.25 in (0.64 cm) and weeding; Ideal for prespaced and electronically cut, screen printed or used in narrow width thermal transfer printing systemsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
63.5 - 88.9 microns
2.50 - 3.50 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2490 psi
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Polypropylene
0.701 kN/m
4.00 pli
Adhesion to ABS
0.701 kN/m
4.00 pli
Adhesion to Acrylic
0.701 kN/m
4.00 pli
Adhesion to Acrylic enamel
0.701 kN/m
4.00 pli
Adhesion to Fruehauf pre-painted panels
0.701 kN/m
4.00 pli
Adhesion to Polycarbonate
0.701 kN/m
4.00 pli
Adhesion to Urethane paints
0.877 kN/m
5.00 pli
Adhesion to Chrome
1.40 kN/m
8.00 pli
Adhesion to Aluminum, alodine
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Descriptive Properties Value Comments
Appearance Dark violet