Material Notes:
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
MD; ASTM D955
Melt Flow 2.8 g/10 min
2.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 26 %
26 %
ASTM D638
Tensile Modulus 1.650 GPa
239.3 ksi
ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F