| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE |
| Manufacturer | Adamas |
| Trade Name | Adalon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adamas Adalon® 600 PTFE, Boro Nitruro.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.15 - 2.16 g/cc | 2.15 - 2.16 g/cc | ASTM D792 |
| Deformation | 2.7 - 3.8 % | 2.7 - 3.8 % | ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 50 - 52 | 50 - 52 | ASTM D2240 |
| Ball Indentation Hardness | 50.0 - 52.0 MPa | 7250 - 7540 psi | ISO 2032 |
| Tensile Strength at Break | 23.0 - 24.0 MPa | 3340 - 3480 psi | ASTM D4745-97 |
| Elongation at Break | 220 - 225 % | 220 - 225 % | ASTM D4745-97 |
| Coefficient of Friction, Static | 0.10 - 0.15 | 0.10 - 0.15 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.820 W/m-K | 5.69 BTU-in/hr-ft²-°F | ASTM C 177 |
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 250 °C | 482 °F | DSC |
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |