| Category | Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled |
| Manufacturer | Adamas |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adamas Rixon 430 PEEK, 30% Carbon Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 - 1.415 g/cc | 1.40 - 1.415 g/cc | ASTM D792 |
| Water Absorption | 0.10 - 0.15 % | 0.10 - 0.15 % | Immersion 24 hrs; ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 100 - 105 | 100 - 105 | ASTM D785 |
| Hardness, Shore D | 88 - 90 | 88 - 90 | ASTM D2240 |
| Ball Indentation Hardness | 410 - 440 MPa | 59500 - 63800 psi | ISO 2032-N961 |
| Tensile Strength at Break | 90.0 - 110 MPa | 13100 - 16000 psi | ASTM D638 |
| Elongation at Break | 5.0 - 7.0 % | 5.0 - 7.0 % | ASTM D638 |
| Tensile Modulus | 1.40 - 1.45 GPa | 203 - 210 ksi | ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 343 °C | 649 °F | DSC |
| Maximum Service Temperature, Air | 250 °C | 482 °F | DSC |
| Minimum Service Temperature, Air | -80.0 °C | -112 °F | DSC |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | ASTM D257 |
| Surface Resistance | 1e+05 | 1e+05 | ASTM D257 |