| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183/A |
| Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 78 | 78 | ISO 868 |
| Tensile Strength at Break | 28.0 MPa | 4060 psi | ISO R 527 |
| Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO R 527 |
| Elongation at Yield | 10 % | 10 % | ISO R 527 |
| Modulus of Elasticity | 4.00 GPa | 580 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | ISO 180/1A |
| Charpy Impact Unnotched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/IeU |
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-2/AF |
| Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | CEI 60093 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 |
| Comparative Tracking Index | >= 600 V | >= 600 V | CEI 60112/Solution A |