| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Mineral Reinforced |
| Manufacturer | Addiplast |
| Trade Name | Addilene |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Addiplast Addilene J 522 M20 Polypropylene Copolymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183/A |
| Melt Flow | 18 g/10 min | 18 g/10 min | ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 68 | 68 | ISO 868 |
| Tensile Strength at Break | 20.0 MPa | 2900 psi | ISO R 527 |
| Tensile Strength, Yield | 25.0 MPa | 3630 psi | ISO R 527 |
| Elongation at Yield | 20 % | 20 % | ISO R 527 |
| Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
| Charpy Impact Unnotched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/IeU |
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | CEI 60093 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 |
| Comparative Tracking Index | >= 600 V | >= 600 V | CEI 60112/Solution A |