| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 88 | 88 | Conditioned; ISO 868 |
| 89 | 89 | ISO 868 | |
| Tensile Strength at Break | 100 MPa | 14500 psi | Conditioned; ISO R 527 |
| 125 MPa | 18100 psi | ISO R 527 | |
| Elongation at Break | 5.0 % | 5.0 % | ISO R 527 |
| 5.0 % | 5.0 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 6.30 GPa | 914 ksi | Conditioned; ISO 178 |
| 7.50 GPa | 1090 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180/1A |
| 11.0 kJ/m² | 5.23 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
| 6.50 J/cm² | 30.9 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/IeA |
| 1.15 J/cm² | 5.47 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ISO 75-2/AF |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| Oxygen Index | 34 % | 34 % | ISO 4589 |
| Glow Wire Test | 960 °C | 1760 °F | CEI 60695/2/1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Conditioned; CEI 60093 |
| 1.00e+13 ohm | 1.00e+13 ohm | CEI 60093 | |
| Comparative Tracking Index | 275 V | 275 V | CEI 60112/Solution A |