Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 103 MPa
14900 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 5.20 GPa
754 ksi
ASTM D790
Compressive Yield Strength 117 MPa
17000 psi
ASTM D695
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
424 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 197 °C
387 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: