Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Flexible Tubing Grade
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical resistance. Ability to be processed at high speed.Example applications: Flexible tubes for air brake system approved by ISO 7628, DIN 73378 (PA11-PHL), NFR 12632, SAEJ 844.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Water Absorption 1.6 %
1.6 %
Melt Flow 3.1 g/10 min

@Load 10.0 kg,
Temperature 235 °C
3.1 g/10 min

@Load 22.0 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa

@Strain 50.0 %
3770 psi

@Strain 50.0 %
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.330 GPa
47.9 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Electrical Properties Metric English Comments
Dissipation Factor 0.000405

@Frequency 1e+6 Hz
0.000405

@Frequency 1e+6 Hz
0.00090

@Frequency 100 Hz
0.00090

@Frequency 100 Hz