| Category | Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled |
| Manufacturer | Arlon |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arlon 55946C028 Silicone Rubber/Fiberglass Laminate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.32 g/cc | 1.32 g/cc | silicone property; Arlon SQA-TMS-024 |
| Thickness | 127 microns | 5.00 mil | side 1; Arlon SQA-TMS-003 |
| 165 microns | 6.50 mil | side 2; Arlon SQA-TMS-003 | |
| 457 microns | 18.0 mil | substrate; Arlon SQA-TMS-003 | |
| 749 microns | 29.5 mil | overall; Arlon SQA-TMS-003 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 55 | 55 | silicone property; ASTM D2240 |
| Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | silicone property; ASTM D412 |
| Elongation at Break | 550 % | 550 % | silicone property; ASTM D412 |
| Adhesive Bond Strength | 0.0483 MPa | 7.00 psi | ASTM D624 |
| Tear Strength | 21.0 kN/m | 120 pli | Die B; silicone property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min @Temperature 204 °C |
2.00 hour @Temperature 400 °F |
|
| 15.0 min @Pressure 0.345 MPa, Temperature 121 °C |
0.250 hour @Pressure 50.0 psi, Temperature 250 °F |
||
| Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Brown |