| Category | Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive |
| Manufacturer | Armstrong Epoxy Adhesives; Resin Technology Group |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Armstrong A-5/E Epoxy Adhesive.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 13000 cP | 13000 cP | Mixed |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 75 | 75 | |
| Tensile Strength, Ultimate | 29.0 MPa | 4200 psi | after optimum cure |
| Elongation at Break | 1.8 % | 1.8 % | |
| Adhesive Bond Strength | 53.8 MPa | 7800 psi | Steel-Steel; after optimum cure |
| 11.4 MPa @Temperature 25.0 °C |
1650 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear | |
| 14.8 MPa @Temperature -54.4 °C |
2150 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear | |
| 17.2 MPa @Temperature 82.2 °C |
2500 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
|
| Glass Transition Temp, Tg | 100 °C | 212 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 93.3 °C | 200 °F | Optimum cure is 1 hr. @ 200°F |
| Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Silver | |
| Mix Ratio | 100/10 | By Weight |