Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall MD-5009 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall MD-5009 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf MD-5009 is a rigid, fitting-grade PVC compound designed for hot spruce/runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which includes color hold, regrind stability and surface appearance. MD-5009 is NSF listed under Standard 14/61 for both potable water and DWV applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D-638
Tensile Modulus 2.90 GPa
420 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D-790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
0.700 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
0.587 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.00 °C
159.8 °F
ASTM D-648
Oxygen Index 38 %
38 %
ASTM D-2863
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 12454
NSF std. 14
Flow Ratio (Distance/Wall Thickness, 390-400°F) 175
Georgia Gulf Test