| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 20% Glass Fiber Reinforced |
| Manufacturer | Barlog Plastics |
| Trade Name | KEBAFORM |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Barlog Plastics KEBAFORM C 2027 POM Copolymer, 20% glass fiber reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
| Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1 |
| Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1 |
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179-1eU |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179-1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Resin Type | POM-GF20 |